用氯化胆碱-草酸从次氧化锌粉尘中梯级分离铟及伴生元素OA
Step-up Separation of Indium and Associated Elements from Zinc Oxide Dust Using Choline-Oxalic Acid Chloride
为高效富集次氧化锌粉尘中的铟并实现伴生元素的定向分离回收,研究采用氯化胆碱-草酸二水合物低共熔溶剂浸出粉尘中的Zn、Fe、Pb、In,并结合"水解脱锌铅—紫外光还原除铁"工艺进行分步除杂.结果表明:在液固体积质量比12 mL/1 g、温度70 ℃、时间6 h的优化浸出条件下,Zn、In、Pb、Fe浸出率分别达95.52%、88.91%、80.82%和89.13%;浸出液通过水解沉淀可脱除Zn/Pb,再经紫外光还原沉淀可脱除Fe;经此分步沉淀除杂处理后,溶液中In质量分数由0.03%提升至1.5%,能成功实现铟的高效富集,以及Zn、Pb、Fe等伴生元素的定向分离回收.
In order to efficiently enrich indium(In)in zinc oxide dust and realize the directional separation and recovery of associated elements,Zn,Fe,Pb and In were leached from the dust by choline chloride-oxalate dihydrate low eutectic solvent,and the"hydrolytic removal of zinc and lead-ultraviolet light reduction iron removal"process was used to remove impurities step by step.The results show that the leaching rates of Zn,In,Pb and Fe can reach 95.52%,88 91%,80.82%and 89.13%,respectively,under the optimal leaching conditions of liquid volume to solid mass ratio of 12 mL/1 g,temperature of 70 ℃ and time of 6 h.Zn/Pb is removed by hydrolytic precipitation,and then Fe is removed by ultraviolet reduction precipitation.After the step-by-step precipitation and impurity removal treatment,the mass fraction of indium in the solution has increased from 0.03%to 1.5%,successfully achieving efficient enrichment of indium and directional separation and recovery of associated elements such as Zn,Pb,and Fe.
张良进;刘勇志;于奇元;龙跃;张玉柱
华北理工大学冶金与能源学院,河北 唐山 063210||中冶检测认证有限公司,北京 100088华北理工大学冶金与能源学院,河北 唐山 063210||华北理工大学现代冶金技术教育部重点实验室,河北 唐山 063210华北理工大学冶金与能源学院,河北 唐山 063210||华北理工大学现代冶金技术教育部重点实验室,河北 唐山 063210华北理工大学冶金与能源学院,河北 唐山 063210||华北理工大学现代冶金技术教育部重点实验室,河北 唐山 063210华北理工大学冶金与能源学院,河北 唐山 063210||华北理工大学现代冶金技术教育部重点实验室,河北 唐山 063210
矿业与冶金
低共熔溶剂次氧化锌粉尘铟梯级提取浸出分离回收
deep eutectic solventzinc oxide dustindiumcascade extractionleachingseparationrecovery
《湿法冶金》 2026 (1)
52-57,6
国家自然科学基金区域创新发展联合基金资助项目(U20A20271).