氟醚唇形油封摩擦磨损及老化性能试验分析OA
Friction,wear and aging performance of fluoroether lip oil seals
针对氟醚橡胶材质的唇形油封,基于多用途传动摩擦试验台,结合唇形油封不同过盈量与耐介质老化时间参数,开展变转速干摩擦试验,分析耐介质老化时间、过盈量对油封安装主轴转矩、振动及摩擦磨损的影响.试验结果表明:在本试验选用的参数范围内,随着老化时间延长,主轴转矩随之降低,振动呈先减后增的趋势;随着过盈量的增大,主轴转矩、振动随之增大;老化时间越长,过盈量越低,油封磨损量越小.此外,随着耐介质老化时间增长,试件摩擦区域表面越光滑,溶胀现象越显著.
Using a multi-purpose transmission friction test bench,variable-speed dry friction tests were conducted on lip-type oil seals composed of fluoroether rubber,with considering different interference levels and media-aging durations.The effects of aging time and interference on spindle torque,vibration,and frictional wear were systematically analyzed.Results show that,within the tested parameter range,spindle torque decreases with prolonged aging time,while vibration initially decreases and subsequently increases.Increasing interference leads to higher spindle torque and vibration.Moreover,longer aging time and lower interference correspond to reduced wear of the oil seal.Surface observations further indicate that extended aging time produces smoother frictional surfaces and more pronounced swelling.
梁校瑞;陈立杉;孟凡明;高致远;杨圣
重庆大学 高端装备机械传动全国重点实验室,重庆 400044重庆长安汽车股份有限公司,重庆 401120中国船舶集团有限公司第705研究所,西安 710077重庆大学 高端装备机械传动全国重点实验室,重庆 400044重庆大学 高端装备机械传动全国重点实验室,重庆 400044
机械制造
油封摩擦磨损耐介质老化氟醚橡胶振动试验
oil sealfriction and wearresistance to medium agingfluoroether rubbervibration test
《重庆大学学报》 2026 (1)
32-39,8
国家自然科学基金资助项目(52175160).Supported by the National Natural Science Foundation of China(52175160).