偏高岭土-水泥基复合砂浆的宏观性能及微观孔结构分析OA
Macroscopic Properties and Micro-pore Structure Analysis of Metakaolin-cement Based Composite Mortar
为了探究不同偏高岭土替代率对水泥基复合砂浆的宏观性能及微观孔结构影响,利用沙漠砂、机制砂、沙漠砂+机制砂分别作为细骨料,以偏高岭土替代部分水泥(0%、3%、5%、7%、9%)制备M10砂浆,并对其进行宏观性能(工作性能、力学性能、抗冻性能)试验,最后通过场发射扫描电镜(SEM)、核磁共振(NMR)对砂浆冻融循环试验后的微观形貌和孔结构进行分析.结果表明:随着偏高岭土掺量增加,3种砂浆的吸水率呈下降趋势,当替代率为9%时,沙漠砂砂浆、机制砂砂浆和混合砂砂浆的吸水率较基准组分别降低6.7%、9.0%和7.2%,而相同替代率下3种砂浆的保水率分别提高13.9%、13.1%和13.8%.力学性能测试表明,砂浆抗折强度随偏高岭土掺量增加呈先升后降趋势,最佳掺量均为5%,在此掺量下28 d龄期的沙漠砂砂浆、机制砂砂浆和混合砂砂浆的抗折强度较基准组分别提升44.4%、42.5%和35.9%.冻融循环试验表明,50次循环后,3种砂浆的强度和质量损失率均在5%替代率时均达到最低值,并呈现先降后升的变化规律.适量的沙漠砂替代机制砂可以提升砂浆的密实程度,从而提高混合砂砂浆的整体性能;此外,适量的偏高岭土可以与水泥产生二次反应生成更多的CSH胶凝,减小砂浆内部的孔隙,促使大孔转变为小孔,进而提升砂浆的各项性能.
To investigate the effects of different metakaolin substitution rates on the macro-performance and micro-pore structure of cement-based composite mortar,this study utilized desert sand,manufactured sand,and a combination of desert sand and manufac-tured sand as fine aggregates.M10 mortar was prepared by partially replacing cement with metakaolin at substitution rates of 0%,3%,5%,7%,and 9%.Macro-property tests were conducted to evaluate the workability,mechanical properties,and frost resistance.Additionally,the microscopic morphology and pore structure of the mortar after the frost resistance test were analyzed using field emission scanning electron microscopy(SEM)and nuclear magnetic resonance(NMR).The results showed that with the increase of the content of metakaolin,the water absorption rates of the three mortars decreased.When the substitution rate was 9%,the water absorption rates of desert sand mortar,manufactured sand mortar and mixed sand mortar decrease by 6.7%,9.0%and 7.2%respec-tively,compared to the reference group.Meanwhile,under the same substitution rate,the water retention rates of the three types of mortar increased by 13.9%,13.1%and 13.8%respectively.Mechanical property tests showed that the flexural strength of mortar in-creased first and then decreased with the dosage of metakaolin,and the optimal dosage of 5%for all types.At this dosage,the flexural strengths of desert sand mortar,manufactured sand mortar and mixed sand mortar at the age of 28 days increased by 44.4%,42.5%and 35.9%respectively,compared to the reference group.The freeze-thaw cycle test showed that after 50 cycles,the strength and quality loss rates of the three kinds of mortars all reached the lowest values when the substitution rate was 5%,exhibiting a pattern of first decreasing and then increasing.An appropriate amount of desert sand instead of manufactured sand could enhance the compact-ness of mortar,thereby improving the overall performance of mixed sand mortar.In addition,an appropriate amount of metakaolin could undergo a secondary reaction with cement to generate more CSH cementitious substances,reducing the internal pores of the mortar,and promoting the transformation of large pores into small ones,thereby enhancing the various properties of the mortar.
魏迎博;周海龙;吴晓宜
内蒙古农业大学水利与土木建筑工程学院,呼和浩特 010018内蒙古农业大学水利与土木建筑工程学院,呼和浩特 010018||内蒙古农业大学旱区水工程生态环境全国重点实验室,呼和浩特 010018内蒙古农业大学水利与土木建筑工程学院,呼和浩特 010018
建筑与水利
偏高岭土替代率沙漠砂砂浆机制砂砂浆混合砂砂浆力学性能工作性能抗冻性能
Metakaolin replacement ratioDesert sand mortarManufactured sand mortarMixed sand mortarMechanical proper-tiesWorkabilityFrost resistance performance
《内蒙古农业大学学报(自然科学版)》 2026 (1)
58-65,100,9
内蒙古自然科学基金项目(2024LHMS05026)内蒙古自治区研究生教育教学改革项目(JGCG2023065)
评论